Gloves - Tables of Properties and Resistances
- Expand All Compress All
General Glove Properties
| Glove | Cost | General Chemical Resistance | Recommended Uses | Disadvantages |
| Latex | low | decent for dilute inorganic solutions | bases, alcohols, dilute water solutions, okay with aldehydes and ketones | poor for most organics |
| Polyvinyl Chloride | low | medium general resistance | strong acids and bases, salts, alcohols, amines, peroxides, water solutions | plasticizers my be stripped, poor for most organics |
| Nitrile | low | some organics | oils, greases, aliphatic chemicals, xylene, perchloroethylene, trichloroethane, toluene, some acids and bases, some biohazardous materials | not good with many ketones, benzene, methylene chloride, and trichloroethane |
| Neoprene | medium | medium general resistance | oxidizing acids, peroxides, hydrocarbons, alcohol, anilines, phenol, glycol, ethers | not good with many chlorinated solvents, esters, ketones, aromatics |
| Viton | extremely high | organic solvents | aromatics, chlorinated solvents, aliphatics and alcohols | poor physical properties, not good with some ketones, esters and amines |
| Butyl | high | polar organics | glycol ethers, ketones, esters | not good with hydrocarbons, halogenated solvents |
| Polyvinyl Alcohol | very high | organics | aliphatics, aromatics, chlorinated solvents, ketones, esters, ethers | Not good with alcohols, acids, bases; glove is destroyed by water |
| Silver Shield | medium | high general resistance | hazmat | poor fit, stiff, easily punctured |
General Glove Resistance
| Chemical Hazard | Latex | Polyvinyl Chloride | Nitrile | Neoprene | Polyethlylene | Viton | Butyl | Polyvinyl Alcohol |
| Dilute Acids | + | + | + | + | | + | + | |
| Alcohols | + | + | + | + | + | + | + | |
| Alkali | + | + | + | + | | + | + | |
| Aromatics | | | | | | + | | + |
| Chlorinated Hydrocarbons | | | + | | | + | + | + |
| Epoxy Resins | | + | + | + | | + | + | |
| Esters | | | | | | | + | |
| Hydrocarbons | | | + | + | | + | + | + |
| Ketones | | | | | | | + | |
| Lacquer Thinners | | | + | + | | + | + | + |
| Oils, Grease | | + | + | + | | + | + | + |
| Petroleum Distillates | | | + | + | | + | + | + |
| PCB's | | | | | | + | |
Glove Suitability for Specific Cleanroom Chemicals
| Chemical Hazard | Latex | Polyvinyl Chloride | Nitrile | Neoprene | Polyurethane | Polyethlylene | Viton (fluoroelastimer) | Butyl | Polyvinyl Alcohol | Silver Shield (norfoil) |
| Acetic Acid | G | F | F | G | F | F | G | G | P | UNK |
| Acetone | F | P | F | F | G | P | P | G | P | G |
| Ammonium Fluoride, 30-79% | G | F | G | F | F | UNK | UNK | UNK | UNK | UNK |
| Ammonium Hydroxide, < 30% | G | G | G | G | F | G | UNK | G | UNK | UNK |
| Ammonium Hydroxide 30-70% | G | F | G | G | F | F | UNK | UNK | P | UNK |
| Aqua Regia | F | F | P | G | P | UNK | UNK | UNK | UNK | UNK |
| Chromic Acid | P | F | F | P | P | P | G | G | P | UNK |
| Freon TMC | F | P | F | P | UNK | UNK | UNK | UNK | G | UNK |
| Freon 113 or TF | P | F | G | G | G | UNK | UNK | UNK | UNK | UNK |
| Hydrochloric Acid < 30% | G | F | G | G | P | F | G | G | P | UNK |
| Hydrochloric Acid 30-70% | G | F | F | G | P | P | UNK | UNK | P | UNK |
| Hydrofluoric Acid < 10% | G | F | G | F | P | F | UNK | UNK | UNK | UNK |
| Hydrofluoric Acid < 50% | F | F | F | F | P | P | UNK | UNK | P | UNK |
| Hydrogen Peroxide | G | G | G | F | UNK | G | G | G | P | UNK |
| Isopropyl Alcohol (2-propanol, Isopropanol) | G | F | G | G | G | G | G | G | UNK | UNK |
| Methyl Alcohol (Methanol) | P | P | P | P | UNK | UNK | G | G | UNK | UNK |
| Methyl Ethyl Ketone | F | P | P | F | G | P | P | P | F | G |
| Methyl Isobutyl Ketone | P | P | P | P | G | P | UNK | UNK | UNK | UNK |
| N-Methyl-2-Pyrrolidone | G | F | P | UNK | F | UNK | UNK | UNK | UNK | UNK |
| Nitric Acid < 30% | G | G | F | G | P | F | G | G | UNK | G |
| Nitric Acid 30-70% | P | P | P | F | P | P | G | G | P | UNK |
| Phosphoric Acid > 70% | F | G | F | G | F | F | G | G | P | UNK |
| Potassium Hydroxide | G | G | G | G | P | F | G | G | P | UNK |
| Propylene Glycol Monomethyl Ether Acetate | G | G | G | G | UNK | UNK | G | G | UNK | UNK |
| Sulfuric Acid 30-70% | G | F | P | G | P | F | G | G | P | G |
| Sulfuric Acid > 70% | P | P | P | F | P | P | F | F | P | UNK |
| Xylenes | P | F | F | P | G | UNK | G | G | UNK | G |
G=GOOD F=FAIR P=POOR UNK=UNKNOWN
Other Websites Containing Glove Suitability Information for Other Chemicals
- http://www.qrpgloves.com/pdfs/spread7.pdf
- http://www.safeskin.com/ChemResist/search.asp?o=1
- http://www.chemrest.com/domesticprep2/All%20Data%20Home%20Page.htm
- http://www.tasco-safety.com/workgloves/chem.html
- http://www2.fpm.wisc.edu/chemsafety/glove%20chemical%20resistance.pdf
- http://www.chemistry.ohio-state.edu/ehs/pdf/select.pdf
- http://ehs.sc.edu/gloves.htm
- Return to Personal Protective Equipment
|